Fractography of Ceramic and Metal Failures

 

 

کتابخانه الکترونیکی دیتا ساینس

شناسه: Ebook-291216.1

عنوان: Fractography of Ceramic and Metal Failures

لینک: https://www.astm.org/DIGITAL_LIBRARY/STP/SOURCE_PAGES/STP827.htm

قیمت: ۱۰۲۰۰ تومان (۱۰ درصد تخفیف اعضاء ویژه)

 

The Symposium on Fractography in Failure Analysis of Ceramics and Metals, sponsored by ASTM Committee E24 on Fracture Testing, was held at ASTM Headquarters, Philadelphia, Pennsylvania, on 29-30 April 1982. J. J. Mecholsky, Jr., Sandia National Laboratories, and S. R. Powell, Jr., Bell Helicopter Company, served as symposium chairmen. This volume, Fractography of Ceramic and Metal Failures, has been edited by Messrs. Mecholsky and Powell.